The veneer after peeling has a high moisture content and can be directly dyed before drying. However, if the raw materials of the veneer are to be stored for use during the off-season of harvesting, drying treatment needs to be carried out after peeling to facilitate storage and prevent mold and decay…
Quality requirements for engineered vendors are required for the quality of rotary cut veneerThe quality of veneer is directly related to the quality of technology wood products. There are several indicators for evaluating the quality of technology wood veneer: veneerthickness deviation, i.e.…
In the production of Engineered veneer, the length of wood segments used for rotary cutting veneer is generally 1900mm, 2300mm, 2600mm, 2900mm, and 3300mm. The production of boards is similar, but special attention should be paid to the following points:1、When rotary cutting, non porous adhesive ta…
The raw materials used in Engineered veneerare mainly single board or thin wood made from logs of ordinary or fast-growing tree species. The manufacturing technology of veneer directly affects the quality, production efficiency, comprehensive utilization rate, and production cost of technologi…
On the transverse plane, many light colored radiating lines can be seen, called rays. The rays originating from the outward extension of primary meristem are called primary rays.…
Natural veneer is taken from logs, and the wood formed during each growing season is called a growth ring, which forms a concentric circle around the pith center on the transverse plane.…